固态锂硫电池电解质及其界面问题研究进展
朱鑫鑫, 蒋伟, 万正威, 赵澍, 李泽珩, 王利光, 倪文斌, 凌敏, 梁成都

Research progress in electrolyte and interfacial issues of solid lithium sulfur batteries
Xinxin ZHU, Wei JIANG, Zhengwei WAN, Shu ZHAO, Zeheng LI, Liguang WANG, Wenbin NI, Min LING, Chengdu LIANG
图5 (a) S/CMK-3(b) 230 ℃热处理后S/CMK-3复合电极的全固态电池充放电曲线[45]
Fig. 5 Charge-discharge curves of all-solid-state batteries with composite electrodes of (a) sulfur/CMK-3 and (b) sulfur/CMK-3 heat treated at 230 [45]