NASICON结构Li1+xAlxTi2-x(PO4)30x0.5)固体电解质研究进展
吴洁, 江小标, 杨旸, 吴勇民, 朱蕾, 汤卫平

Progress of NASICON-structured Li1+xAlxTi2-x(PO4)3 (0 x 0.5) solid electrolyte
Jie WU, Xiaobiao JIANG, Yang YANG, Yongmin WU, Lei ZHU, Weiping TANG
图11 Li/Al2O3@LATP@Al2O3/LiLi/LATP/Li对称电池在0.01 mA/cm2电流密度下的电化学行为以及LATP/Li界面示意图[116]
Fig.11 Electrochemical behavior of Li/Al2O3@LATP@Al2O3/Li and Li/LATP/Li symmetrical cell at a current density of 0.01 mA/cm2 and schematic diagram of LATP/Li interface with and without Al2O3[116]