NASICON结构Li1+xAlxTi2-x(PO4)30x0.5)固体电解质研究进展
吴洁, 江小标, 杨旸, 吴勇民, 朱蕾, 汤卫平

Progress of NASICON-structured Li1+xAlxTi2-x(PO4)3 (0 x 0.5) solid electrolyte
Jie WU, Xiaobiao JIANG, Yang YANG, Yongmin WU, Lei ZHU, Weiping TANG
图8 (a) 全固态电池LiCoO2/LATP/Li结构示意图;(b)(c) 循环50圈后,LiCoO2/LATP界面的EDS线扫和元素mapping[105]
Fig.8 (a) schematic diagram of all-solid LiCoO2/LATP/Li cell; (b)(c) compositional EDS line scan and elemental mapping data of LiCoO2/LATP interface after 50 cycles[105]