NASICON结构Li1+xAlxTi2-x(PO4)30x0.5)固体电解质研究进展
吴洁, 江小标, 杨旸, 吴勇民, 朱蕾, 汤卫平

Progress of NASICON-structured Li1+xAlxTi2-x(PO4)3 (0 x 0.5) solid electrolyte
Jie WU, Xiaobiao JIANG, Yang YANG, Yongmin WU, Lei ZHU, Weiping TANG
图2 (a) 在实验室(实心圆)和旋转参照系(空心圆)下研究的Li1.5Al0.5Ti1.5(PO4)37Li NMR自旋-晶格弛豫(SLR)速率R1RArrhenius曲线[70](b) LATP陶瓷电导率的Arrhenius曲线(插图:在T >135 ℃时,Li+可能的主要传导途径)[71]
Fig.2 (a) Arrhenius plot of 7Li NMR SLR rates R1 and R of Li1.5Al0.5Ti1.5(PO4)3 investigated in laboratory (filled circles) and rotating frame of reference (empty circles), respectively[70]; (b) Arrhenius plot of conductivity of LATP ceramic (inset:possible predominant Li conduction pathway at T > 135 )[71]