钠离子电池层状氧化物正极:层间滑移,相变与性能
刘欢庆, 高旭, 陈军, 尹首懿, 邹康宇, 徐来强, 邹国强, 侯红帅, 纪效波

Layered oxide cathode for sodium ion batteries: Interlayer glide, phase transition and performance
Huanqing LIU, Xu GAO, Jun CHEN, Shouyi YIN, Kangyu ZOU, Laiqiang XU, Guoqiang ZOU, Hongshuai HOU, Xiaobo JI
图7 (a) Na0.66Co0.5Mn0.5O2电极的原位XRD[88](b) 2.04.4 V范围内,P2/O3/O1NaxNi1/3Co1/3Mn1/3O2的原位XRD[89](c) Na2/3Ni1/3-xFexTi2/3O2的原位XRD表征[47](d) 2.54.0 V范围内,P2/O3NaxNi0.2Fex-0.4Mn1.2-xO2原位XRD[90]
Fig.7 (a) in-situ XRD patterns of the Na0.66Co0.5Mn0.5O2 electrodes at various states[88]; (b) in operando HEXRD patterns of P2/O3/O1-NaxNi1/3Co1/3Mn1/3O2 cathodes within 2.04.4 V[89]; (c) in-situ XRD characterization of Na2/3Ni1/3-xFexTi2/3O2 electrodes[47]; (d) in-situ XRD patterns of P2/O3-NaxNi0.2Fex-0.4Mn1.2-xO2 over a voltage range of 2.54.0 V[90]