以废旧锰酸锂正极为原料制备Li0.25Na0.6MnO2钠离子电池正极材料的研究
聂雪娇, 郭晋芝, 王美怡, 谷振一, 赵欣欣, 杨旭, 梁皓杰, 吴兴隆

Using spent lithium manganate to prepare Li0.25Na0.6MnO2 as cathode material in sodium-ion batteries
Xuejiao NIE, Jinzhi GUO, Meiyi WANG, Zhenyi GU, Xinxin ZHAO, Xu YANG, Haojie LIANG, Xinglong WU
图5 (a) LNMO材料的不同扫速的CV曲线;(b) LNMO材料各峰的峰电流和扫速的平方根(v1/2)的线性拟合,电压范围为1.64.2 V
Fig.5 (a) CV curves of LNMO materials at different sweep speeds; (b) linear fitting of the peak current and the square root (v1/2) of the sweep speed of each peak of LNMOmaterial, with a voltage range of 1.64.2 V